Major Edges | ||
---|---|---|
K | 4493 | |
L2 | 407 | |
L3 | 402 | |
M23 | 32 |
Minor Edges | ||
---|---|---|
L1 | 501 | |
M1 | 54 |
Sc2O3 thin film_0-0950eV
- Material Analyzed:Sc2O3
- Related Elements:Scandium, Oxygen
- Data Contributor:Gatan
- Beam energy (keV):200
- Nominal energy range (eV):0 - 950
- Collection semi-angle effective (mrad):100
- Notes:
Serial EELS; zero-loss peak intensity = 7.98e8; total elastic int. / zero-loss int. = 0.34; gain change factor = 727; 35 sweeps 30 ms dwell